Title Hollow cone dark field observation of a 3D NAND flash memory using a 120 kV TEM
Details HTD-TEM-E032
Overview “Hollow cone dark field observation of a 3D NAND flash memory using a 120 kV TEM“

Plane view TEM of 3D NAND flash memory was performed on 120 kV TEM. While concentric multi-layer was clearly observed inside memory cell on bright field image, grains of tungsten gate electrode and poly-crystalline Si layer were vividly visualized on hollow cone dark field image.

Further details can be found on our membership website with data library.
Looking forward to your joining.
About our membership site, see https://www.hitachi-hightech.com/global/en/support/sinavi/
Related links (products)
Product type ・Focused Ion Beam Systems (FIB)
・Transmission Electron Microscopes (TEM)
Field 1 Materials science
Field 2 Semiconductors (incl. materials) / Devices / Components / Displays & Lighting
Information type Technical Data / Data Sheet
Issue date 2019/11/11
Inquiry Inquiry
No. HTD-TEM-E032