“TEM observation of cellulose nanofibers treated with ionic liquid”
Cellulose nanofibers were observed by TEM using ionic liquid. Cellulose nanofibers suspension was mixed with ionic liquid and then negatively stained. Each fiber can be clearly observed at high magnification.