“Cryo-transfer observation of liposomes using a 120 kV“
Empty and drug-loaded liposomes embedded in rapidly frozen vitreous ice were observed at -175 ℃ using a cryo-transfer holder. Their shape, membrane structure, and loaded drugs were clearly visualized under low dose conditions using high-sensitivity CMOS camera.