The increasing demand for high quality Nd-Fe-B magnets used in electric vehicle motors requires their exact control, observation and evaluation of the nanostructure, composition and magnetic properties at crystal grain size level. This data sheet presents the observation results of a hot-deformed Nd-Fe-B permanent magnet. The nano-structure, composition and properties of its crystals and grain boundaries were observed with SEM and magnetic force microscopy (MFM) after the flatmilling® process. |