Title | Characterization of the behavior of cokes in zeolite with SU9000 (1) ~ Surface… |
---|---|
Details | HTD-SEM-E033 |
Overview | Characterization of the behavior of cokes in zeolite with SU9000 (1) ~ Surface observation of zeolite particles ~ |
Product type | Field Emission Scanning Electron Microscopes (FE-SEM) |
Field 1 | Materials science |
Field 2 | Nanomaterials / Catalysts / Battery materials / Composite materials / Crystals |
Information type | Technical Note |
Issue date | 2016/12/18 |
Inquiry | Inquiry |
No. | HTD-SEM-E033 |