| Overview |
”Detection of Cathodoluminescence using the UVD”
White phosphor particles were observed and analyzed using various signals. cathodo luminescence image shows the presence of particles of different luminescent sate. EDX result suggests less Mn concentration in bright particles than in dark ones.