| Overview |
”3D structural analysis of Phosphor Materials for White LED in resin with SU5000 and Gatan 3View® 2XP”
1,348 Serial cross-sectional images of resin-embedded white LED phosphors were automatically acquired using Serial Block Face SEM. UVD images depicted phosphors as white particles while resin as black background. 3D reconstruction using an image processing software, Image-Pro, revealed phosphor shape, size, and distribution. Green-colored particles have characteristic shapes (60 mm or more in outside diameter).
Further details can be found on our membership website with data library. Looking forward to your joining. About our membership site, see https://www.hitachi-hightech.com/global/science/guide/ |