“Pore size distribution measurement of alumite sulphate”
Pore size distribution (around 10 nm) of alumite sulphate was automatically measured for a high resolution SEM image using an image analysis software. Pores selected in the SEM image can be linked to the histogram of mean diameter. Also, pores constituting a specified bin in the histogram can be located in the SEM image.