Title Resolving Individual Magnetic Domains in Single-Crystal ε-Fe2O3 via
Details HTD-AFM-E011
Overview Resolving Individual Magnetic Domains in Single-Crystal ε-Fe2O3 via High-Sensitivity in vacuo Magnetic Force Microscopy
Product type Atomic Force Microscopes (AFM)
Field 1 Materials science
Field 2 Metals / Magnetic materials
Information type Technical Data / Data Sheet
Issue date 2020/04/21
Inquiry Inquiry
No. HTD-AFM-E011